Silicon carbide pipes are also known as silicon ceramic pipes, which belong to the refractory pipe family. This kind of pipe is made of clay bonded silicon carbide material, which has good wear resistance, heat resistance, corrosion resistance and high temperature performance. Silicon carbide pipe is the ideal lining material of smelting steel industry, because it has the advantages of high temperature resistance, good slag erosion resistance, high strength and long service life.
Product Parameters
Chemical Index |
Silicon Carbide Pipe |
Bulk density(g/cm3) |
Porosity (%) |
Porosity (%) |
<0.1 |
Bending strength(MPa) |
250(20ºC) |
280(1200ºC) |
Thermal conductivity(W/MK) |
45(1200ºC) |
Thermal expansion(20-1000ºC) 10-6k-1 |
4.5 |
Max. working temperature(ºC) |
1380 |
PH Resistance |
EXCELLENT |
Moh's scale of thermal expansion |
13 |
Feature
1, Moulding: Cold isostatic pressing(CIP)
2, Sintering: GPSN/RSSN
3, High strength and good compactness
4, Low thermal expansion coefficient
5, Excellent thermal shock resistance
6, No wetting by molten aluminum and non-ferrous metal
7, Good corrosion resistance
Detailed Photos
Product Description
Color
Black Grey
Application
Industrial Ceramic,Mechanical Wear Resistant Indus
Density
3.1g/cm3
Size
Accept Customized
Content
98%
Max. Working Temperature
1600 Degree Celsius
Characteristic
Good Thermal Conductivity
Advantage
High Strength,High Hardness
Purpose
High Effeciency of Heat-Conduction
Usage
Industrial Ceramic, Production of Aluminum, Coppe
Function
Used in Tunnel Kiln,Shuttle Kiln and Roller Kiln
Transport Package
Wooden Case
Specification
According Customer Request
Origin
Liao yang, China
HS Code
6909320000
Performance for Silicon Carbide Ceramic :
Item |
Unit |
SiC |
SSiC |
Purity |
% |
≥90 |
≥98 |
Density |
g/cm3 |
3.05 |
3.1 |
Shore Hardness |
HS |
110-125 |
120-130 |
Elastic Modulus |
Mpa |
4.12×105 |
4.10×105 |
Poisson's Ratio |
- |
0.15 |
0.16 |
Tensile Strength |
Mpa |
2.75×102 |
2.8×102 |
Bending Strength |
Mpa |
4.41×102 |
4.9×102 |
Compression Strength |
Mpa |
2.94×102 |
3.0×102 |
Thermal Conductivity |
W/m.k |
141 |
147 |
Coefficient of Thermal Expansion |
1/ °C |
4.3×10-6 |
4.0×10-6 |
Heat Resistance |
- |
1600°C |
1650°C |
Acid Resistance |
- |
5 times higher than the usual TC |
Resist al chemical media |